1-4 of 4 Search Results for

EMPIRE CF-3

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1964) 13 (10): SS-161.
Published: 01 October 1964
... EMPIRE CF-3 is an austenitic chromium-nickel stainless steel casting alloy recommended for welded fabrications because of freedom from carbide precipitation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1972) 21 (8): SS-278.
Published: 01 August 1972
... in induction furnaces where the ultimate in composition and pouring temperature control is possible. Corrosion Resistance: In general, EMPIRE IS040 has superior corrosion resistance to the standard AC1 CF-8 and CF-8M alloys and, in some areas, it is equal to the standard ISO- (CN-7M) alloy which...
Journal Articles
Alloy Digest (1957) 6 (9): SS-61.
Published: 01 September 1957
... EMPIRE CF-3M is a superior stainless steel casting alloy recommended for welded fabrications because of freedom from carbide precipitation. It is equivalent to A. C. I. CF-4M (American Casting Institute designation). This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... 138000 188000 118000 173000 15 14 53 45 Copyright ┬ę ASM International┬« 1996DOI: 10.31399/asm.ad.ss0273 Table 3 - CORROSION RATE OF THREE STAINLESS STEELS 48-Hour Corrosion Rate, mpy 20% Nitric Brinell Acid at Cast Alloy Hardness 2OOoF (930C) CA-l 5 430 8 277 59 IS0450 293 2 387 2 CF-8 163 1 5% Sulphuric...