Alloy Digest (1955) 4 (1): SS-23.
Published: 01 January 1955
... EME is an austenitic nickel-chromium-tungsten-columbium steel having good strength and ductility at 1200 F and excellent forgability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (1966) 15 (11): SA-204.
Published: 01 November 1966
... HECLA EM, 20 is an iron-nickel-cobalt-chromium austenitic alloy steel having high oxidation and scaling resistance. It is recommended for high temperature service and medium loads up to 2000 F, such as turbine blading, jet engine exhaust stacks and combustion chambers. This datasheet provides...
Journal Articles
Alloy Digest (1989) 38 (7): P-6.
Published: 01 July 1989
... as fracture toughness. It also includes information on casting. Filing Code: P-6. Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International amorphous castability elasticity fracture toughness GRILON...
Journal Articles
Alloy Digest (1989) 38 (8): P-7.
Published: 01 August 1989
..., and tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: P-7. Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International castability elasticity...
Journal Articles
Alloy Digest (1989) 38 (10): P-11.
Published: 01 October 1989
... GRILON ELX23NZ is a thermoplastic polyamide elastomer with both rigid and elastomeric components. This datasheet provides information on physical properties, and tensile properties as well as fracture toughness. Filing Code: P-11. Producer or source: EMS-American Grilon Inc.. Producer or Source...
Journal Articles
Alloy Digest (1989) 38 (12): Cp-4.
Published: 01 December 1989
.... Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International castability fracture toughness GRILON PV-15H hardness physical properties tensile properties GRILON PV45H Filing Code: Composite Cp-4...
Journal Articles
Alloy Digest (1990) 39 (6): Cp-8.
Published: 01 June 1990
... on casting. Filing Code: Cp-8. Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International castability fracture toughness GRILON PMV-4H hardness physical properties tensile properties GRILON PMV-4H...
Journal Articles
Alloy Digest (1990) 39 (12): Cp-12.
Published: 01 December 1990
.... Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International castability chemical composition fracture toughness GRILON PV-3H hardness physical properties tensile properties Filing Code: Composite...
Journal Articles
Alloy Digest (1989) 38 (6): P-4.
Published: 01 June 1989
..., and tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: P-4. Producer or source: EMS-American Grilon Inc.. Producer or Source: EMS-American Grilon Inc. Copyright © ASM International® 1996 1996 ASM International castability elasticity GRIVORY G...
Journal Articles
Alloy Digest (1989) 38 (3): P-1.
Published: 01 March 1989
... and Drug Administration (FAD) requirements for direct food contact. It has excellent transparency in thin sections. Grilon is a registered a-ademark of EMS- Chemie AG, Zurich, Switzerland. ChemicalCharacterization: Long-chain synthetic resin with the general formula [-NH-(CI-IJ,-CO-]n Physical Properties...
Journal Articles
Alloy Digest (2011) 60 (9): SA-632.
Published: 01 September 2011
... is a registered trademark of Industeel. CarElso is a patented alloy. Table 2 Suitable filler metals for CarElso 70 (355) SMAW GMAW FCAW SAW Wire Flux Boehler Fox Ev 50 EM K7 EM S3 ESAB OK 48.00 OK 12.51 OK 15.00 OK 15.00S OK 10.71 Lincoln Excalibur 7018 SuperArc L-56 Outershield 75C Lincolnweld L-56 880M...
Journal Articles
Alloy Digest (1978) 27 (2): TS-330.
Published: 01 February 1978
... I I I , ,i 1 1 I I 1 200 300 400 500 Em 760 em 900 Iwo 1100 1200 TEMPERING TEMPERATURE. F Fig. 1 - Effects of wstenitizing and tampering temperatures on hardness. Heat Treatment: Critical Temperature: On heating at a moderate rate, the first appearance of austenite (Acl) is at 14800F. Annealing...
Journal Articles
Alloy Digest (2011) 60 (10): SA-635.
Published: 01 October 2011
... Industeel France 71202 Le Creusot Cedex, France Tel: +33 3 85 80 55 35 Fax: +33 3 85 80 56 99 www.industeel.info ISSN: 002-614X SA-635B Table 2 Non-exclusive list of suitable filler metals SMAW GMAW FCAW SAW Wire Flux BOEHLER Fox Ev 50 EM K7 EM S3 ESAB OK 48.00 OK 12.51 OK 15.00 OK 15.00S OK 10.71...
Journal Articles
Alloy Digest (2020) 69 (2): SS-1315.
Published: 01 February 2020
... Rating Moderate Good Moderate Restricted Moderate Restricted Moderate Restricted Restricted Machinability CarTech 1.4418 Stainless is also offered as an enhanced machining variant, CarTech 1.4418 EM Stainless, which obtains an enhanced machinability characteristic through controlled addition of sulfur...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... salt at approximately 1000°F, held until ness is Brinell20 l-235. temperature is uniform and then cooled in still air. When Stress Relieving: When heavy machining cuts are em- salt quench is not available, a skilled heat treater may ployed the resultant stresses may be relieved by heating quench in oil...
Journal Articles
Alloy Digest (1983) 32 (12): SA-396.
Published: 01 December 1983
... on the base metal. Specific&on Equivalents: AMS 6265. Military: MIL-S-7393. The following industry specifications are offered for general familiarization and should not be considered a complete listing: 299-947-032 (Bell Helicopter). EMS-56279 (Garrett Turbine). BMS 7-249 (Boeing). EMS 65002 & 65005 (Detroit...
Journal Articles
Alloy Digest (2001) 50 (11): Ni-574.
Published: 01 November 2001
... Equivalents: AECMA Designation NI-PH1302 PrEN 2193-2195, 2959, 2960, and 3220 AlliedSignal EMS 55388, 55467 Allison EMS 73111 AMS 5544, 5704, 5706-5709, and 5828 Dresser Rand 099-503 General Electric C50TF90 MTU MTS 1103 Pratt & Whitney PWA 1016, 1007, and CPW-203 Rolls-Royce MSSR 7034, 7192, 7220, and 7250...
Journal Articles
Alloy Digest (1993) 42 (7): SA-465.
Published: 01 July 1993
... nitrogen. The first Super 9% Cr steel was originally approved and developed for superheaters and reheat superheaters. Chemical Composition , Wt. %: EM 12 Carbon 0.015 Manganese 0.80-1.30 Phosphorus 0.030 Sulfur 0.030 Silicon 0.20-0.65 Chromium 8.5-10.50 Molybdenum 1.70-2.30 Nickel 0.030 Aluminum 0.025...
Journal Articles
Alloy Digest (1997) 46 (4): Ni-524.
Published: 01 April 1997
... temperamre. W/m. K 14.6 Magnetic aaraction None NOTE Typical values to guide alloy selection but are not a guar- antee of minimum or maximum ) ) - I - , - TCR VS. HEAT-TREAT TEMPERATURE 25Deg.cto105~.c I I Table 1 Typical Mechanical Properties couadkd Em-IkEed Table 2 Product Availability of Evanohm Fl from...
Journal Articles
Alloy Digest (1963) 12 (11): Cu-135.
Published: 01 November 1963
... Copper) Amphos is a phosphorized oxygen-free copper having free-scaling properties, freedom from hydrogen em- brittlement, improved cold workability, and desirable high softening temperature. *Registered Composition: Physical Constants: Phosphorus Antimony Typical 0.005-0.015 & 0.015-0.025 0.0005...