Alloy Digest (1991) 40 (2): SS-519.
Published: 01 February 1991
... ELMAX is a high-chromium/vanadium/molybdenum alloyed die steel. Powder metallurgy processing results in a unique combination of high wear and corrosion resistant properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It...
Journal Articles
Alloy Digest (2000) 49 (4): SS-778.
Published: 01 April 2000
... scale, which minimizes tool and machine wear, and sur- faces that are free from decarburization. Applications: Typical applications include holders/bolsters for plastic molds. RAMAX S in combination with Stavax ESR or Elmax as insert material gives a completely corrosion resistant mold. (See Alloy...