Skip Nav Destination
Close Modal
Search Results for
ELEKTRON QH21A
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
ELEKTRON QH21A
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1979) 28 (1): Mg-72.
Published: 01 January 1979
... ELEKTRON QH21A is a magnesium-base casting alloy developed to meet the ever increasing requirements for casting alloys to operate at elevated temperatures. It is of particular interest to designers and stress engineers for highly stressed components operating at temperatures up to 480 F (250 C...
Abstract
View article
PDF
ELEKTRON QH21A is a magnesium-base casting alloy developed to meet the ever increasing requirements for casting alloys to operate at elevated temperatures. It is of particular interest to designers and stress engineers for highly stressed components operating at temperatures up to 480 F (250 C), especially where pressure tightness is a requirement. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Mg-72. Producer or source: Magnesium Elektron Inc..