Alloy Digest (2015) 64 (9): Mg-80.
Published: 01 September 2015
... Elektron Wrought Products, North America Copyright ┬ę ASM International┬« 2015 2015 ASM International bend strength castability chemical composition compressive strength corrosion-resistant alloys creep properties elasticity ELEKTRON EQ2 hardness heat treatability high-temperature alloys...