1-7 of 7 Search Results for

ELECTRALLOY NITRONIC 60

Sort by
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
... Electralloy Nitronic 60 is an alloy with excellent uniform corrosion resistance, outstanding galling resistance, high strength, and good high-temperature oxidation resistance. The alloy retains toughness at low temperature. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2018) 67 (10): SS-1295.
Published: 01 October 2018
... Resistance. This material exhibits excellent resistance to wear in sliding metal-to-metal contact superior to type 410 stainless steel, 17-4 precipi- tation hardening stainless steel, or type 304. If galling persists, Electralloy s Nitronic 60 should be considered. Product Forms Available Nitronic 33...
Journal Articles
Alloy Digest (2018) 67 (11): SS-1297.
Published: 01 November 2018
... Electralloy Nitronic 40 is an austenitic, high-strength, corrosion-resistant steel that serves as an alternative to conventional 300 and 400 series stainless steels. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low...
Journal Articles
Alloy Digest (2013) 62 (4): SS-1142.
Published: 01 April 2013
... Electralloy’s Nitronic 33 is a nitrogen strengthened austenitic stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
... and corrosion resistance as well as forming and joining. Filing Code: SS-931. Producer or source: G.O. Carlson Inc., Electralloy. Producer or Source: G.O. Carlson Inc., Electralloy Copyright © ASM International® 2005 2005 ASM International Carlson Nitronic 33 chemical composition corrosion...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
... CARLSON ALLOY NITRONIC 60 is a galling- and wear-resistant austenitic stainless steel that provides a significantly lower-cost alternative to cobalt-bearing and high-nickel alloys. Corrosion resistance is superior to 304 in most media. Approximately twice the yield strength of 340 and 316...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1228.
Published: 01 October 2015
... temperatures in severe seacoast atmospheres. Specification Equivalents: UNS S21900 ASTM A182, A269, A276, A312, A314, A473, A479, A580, A666, A813, A814, A943, A965, A988 AMS 5561, 5562, 5595, 5656 AS/EN/JISQ 9100: 2009 General Characteristics: Electralloy s Nitronic 40 is a nitrogen strengthened austenitic...