1-9 of 9 Search Results for

ELECTRALLOY NITRONIC 50

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... Electralloy Nitronic 50 provides a combination of corrosion-resistance wear and strength not found in other stainless steels. High-speed (HS) Nitronic 50 has a yield strength that is 3 to 4 times that of type 316 stainless steel. This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1294.
Published: 01 September 2018
... Electralloy Nitronic 32 was created to match AISI Type 304 Stainless Steel in corrosion with twice the yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing...
Journal Articles
Alloy Digest (2018) 67 (11): SS-1297.
Published: 01 November 2018
... Electralloy Nitronic 40 is an austenitic, high-strength, corrosion-resistant steel that serves as an alternative to conventional 300 and 400 series stainless steels. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low...
Journal Articles
Alloy Digest (2018) 67 (10): SS-1295.
Published: 01 October 2018
... Electralloy Nitronic 33 was created with a high-yield strength, excellent toughness, and ductility. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (2013) 62 (4): SS-1142.
Published: 01 April 2013
... Electralloy’s Nitronic 33 is a nitrogen strengthened austenitic stainless steel. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
... Electralloy Nitronic 60 is an alloy with excellent uniform corrosion resistance, outstanding galling resistance, high strength, and good high-temperature oxidation resistance. The alloy retains toughness at low temperature. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
... and corrosion resistance as well as forming and joining. Filing Code: SS-931. Producer or source: G.O. Carlson Inc., Electralloy. Producer or Source: G.O. Carlson Inc., Electralloy Copyright © ASM International® 2005 2005 ASM International Carlson Nitronic 33 chemical composition corrosion...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
... strength, min, MPa (ksi) 655 (95) Yield strength (0.2% offset), min, MPa (ksi) 345 (50) Elongation in 2 in., (or 4D), min, % 35 Hardness Brinell (HB), max 241 Rockwell B (HRB), max 100 Galling and Wear Resistance: Due to its grain structure, the galling resistance of Nitronic is superior to that of any...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1228.
Published: 01 October 2015
... temperatures in severe seacoast atmospheres. Specification Equivalents: UNS S21900 ASTM A182, A269, A276, A312, A314, A473, A479, A580, A666, A813, A814, A943, A965, A988 AMS 5561, 5562, 5595, 5656 AS/EN/JISQ 9100: 2009 General Characteristics: Electralloy s Nitronic 40 is a nitrogen strengthened austenitic...