Alloy Digest (2009) 58 (12): Cu-776.
Published: 01 December 2009
... ELECTRALLOY EC63000 and EC63200 are age-hardenable nickel-aluminum-bronze alloys with strength and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well...