Alloy Digest (2010) 59 (6): SS-1069.
Published: 01 June 2010
... Electralloy EC926 Mo is a solution strengthened, austenitic stainless steel alloy providing excellent resistance to aqueous corrosion, coupled with good strength and pitting resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...