Alloy Digest (1992) 41 (2): Cp-20.
Published: 01 February 1992
... ELECTRAFIL G-50/SS/5/FR has a 5% stainless steel fiber loading in a flame retardant modified polycarbonate matrix. It has excellent electrical conductivity and ease of processing. This datasheet provides information on tensile properties, and compressive and shear strength as well as fracture...