1-20 of 34 Search Results for

EB ALLOY

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1969) 18 (4): TS-217.
Published: 01 April 1969
... EB alloy is a high-carbon chromium alloy steel for general hot-work applications. It possesses good compressive strength and hot mechanical properties. It is recommended for hot header and gripper dies, shear blades, hot rivet sets, forging dies, cold forming and embossing dies. This datasheet...
Journal Articles
Alloy Digest (1988) 37 (6): Ta-10.
Published: 01 June 1988
... BIQWT - DATA ON WORlD WIM METALS AND ALLOYS o- 19ss.AlbyDipl.lncc.Auri@uraemd. hbliskd by: Alloy w Inr lSSN:OO2dl4X 27 c4llGeld strsn L&Z. shown ore *pieo. not 10 be used Oran#e. Nev Jy 07050 for #p6#cdm or Jii &sign (201) 677-9161 TANTALUM (Commercially Pure Tantalum) Two grades of Tantalum, EB...
Journal Articles
Alloy Digest (1971) 20 (9): SS-260.
Published: 01 September 1971
... UNILOY EB 26-1 is a stainless steel alloy produced by the electron-beam refining (EBR) process. It is an extremely high-purity ferritic stainless steel, having an attractive combination of strength, ductility, fabricability, and corrosion resistance. This datasheet provides information...
Journal Articles
Alloy Digest (2005) 54 (9): Al-397.
Published: 01 September 2005
... and 7075-T6511. The EXCO test (ASTM G 34, Standard Test Method for Exfoliation Corrosion Susceptibility in 2XXX and 7XXX Series Aluminum Alloys) give a rating of EB (moderate exfoliation) for 7055-T6511 and T74511 compared to ED (very severe exfolia- tion) for 7178-T6511 and 7075-T6511. Results from ANCIT...
Journal Articles
Alloy Digest (2015) 64 (11): CS-193.
Published: 01 November 2015
...@asminternational.org Published by ASM International® :: Data shown are typical, not to be used for specification or final design. Ancorsteel is a registered trademark of Hoeganaes Corp. Fig. 1 The effects of compaction pressure on green properties, 0.75% ethylene bis-stearamide (EBS) DOI: 10.31399/asm.ad.cs0193 ISSN...
Journal Articles
Alloy Digest (2018) 67 (1): SA-809.
Published: 01 January 2018
.... Table 1 Sieve distribution, wt.% mm (in.) US standard mesh +0.25 (+0.01) (+60) Trace +0.15 (+0.006) (+100) 10 0.15/+0.045 ( 0.006/+0.002) ( 100/+325) 70 0.045 ( 0.002) ( 325) 20 Fig. 1 The effects of compacting pressure on green properties. 0.75% ethylene bis-stearamide (EBS) DOI: 10.31399...
Journal Articles
Alloy Digest (2015) 64 (4): Al-442.
Published: 01 April 2015
.... Copyright © 2015, ASM International®. All rights reserved. Corrosion: Alcoa guarantees an accelerated test exfoliation rating of EB or better for 7150-T7751 plate and 7150-T77511 extrusions, based on the 48-hour ASTM G34 EXCO test. This performance level is equivalent to other 7XXX-series alloys...
Journal Articles
Alloy Digest (2016) 65 (10): Al-447.
Published: 01 October 2016
... (ksi in.) SCC min per ASTM G47, ST orientation, MPa (ksi) EXCO rating per ASTM G34 Density, kg/m3 (lb/in.3) Young s modulus, E, L orientation, GPa (106 psi) Young s modulus compression, Ec, L orientation, GPa (106 psi) 25.4 (1.0) 572 (83) 545 (79) 11 30 (27) Better or equal to EB 2850 (0.103) 70.3...
Journal Articles
Alloy Digest (2015) 64 (10): CS-192.
Published: 01 October 2015
... pressure on green proper- ties. 0.75% ethylene bis-stearamide (EBS) Fig. 4 Sintered tensile properties. Composition: All mixes contain 0.75 wt.% ethylene bis-stearamide (EBS). Sintered in 90% nitrogen, 10% hydrogen atmosphere at 1120 °C for 30 min. ...
Journal Articles
Alloy Digest (2004) 53 (5): Al-388.
Published: 01 May 2004
.... Alcoa guarantees an accelerated test exfoliation rat- ing of EB or better for 7150-T7751 plate and 7150-T77511 extrusions, based on the 48 h ASTM G 34 EXCO test. This performance level is equivalent to other 7xxx series alloys in an exfoliation-resistant T76 con- dition. Photographs displaying...
Journal Articles
Alloy Digest (2007) 56 (5): Al-403.
Published: 01 May 2007
... Resistance to SCC, LT direction Alloy Temper MPa ksi EXCO rating(a) 7449 T79511 300(b) 44(b) Better or equal to EC 7175 T6511 285(c) 41(c) Better or equal to EB L, longitudinal; T, transverse. (a) Exfoliation corrosion susceptibility, ASTM G 34. (b) 20 days exposure. (c) 30 days exposure Table 3 Guaranteed...
Journal Articles
Alloy Digest (2020) 69 (2): Ti-163.
Published: 01 February 2020
... by single melt electron beam (EB) processing, or in a multiple melting practice with a final vacuum arc remelting (VAR) processing step. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1971) 20 (9): Be-1.
Published: 01 September 1971
... *Prefatigue cracked. **Unnotched. Short transverse 68 Short transverse 44 Table 3 - DESIGN TYPE PROPERTIES OF ANNEALED SHEET (Sheet thickness 0.040-0.140 in.) property Direction E,* Eb* - - Tensile strength, pn L 44000 47000 T 44000 47000 Yield strength (0.2% offset), psi L 31000 33000 T 31000 33008...
Journal Articles
Alloy Digest (1996) 45 (10): Fe-113.
Published: 01 October 1996
... stainless steel. The material can be joined by TIG. EB. and resistance welding as well as by brazing and soft-solder technique. The heat tmaanent of Precision C can be adjusted to produce the desired value for the thennoelastic coefficient at or near zero. The elevated sangtb in the heat-treated temper...
Journal Articles
Alloy Digest (1998) 47 (2): SA-493.
Published: 01 February 1998
..., 4774 EB 1469 213 10.9 36.7 I207 175 15.5 41.8 1076 156 162 55.2 Heat Treatment: Cdkd~P93T AC3 738 1360 k3 r-7 1340 4 449 840 Ar, 382 720 A~ealing of FX-XTRA or FS after hardening. Charge into a furnace that is at 3 16 C (600 F) or lower. Heat evenly at a rate of 93 C (200 F) per hour to 782-793 C...
Journal Articles
Alloy Digest (2011) 60 (1): Fe-153.
Published: 01 January 2011
... to 150 ºF). Precision C can be readily formed from the annealed temper. It has a work hardening rate similar to austenitic stainless steel. The material can be joined by TIG, EB, and resistance welding as well as by brazing and soft solder techniques. The heat treatment of Precision C can be adjusted...
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... 203 11.7 649 1200 23.0 I33 816 1500 252 14.6 Autogenous, high-power density joining processes such as elec- tron beam (EB) and laser welding should be used with caution due to the low ferrite number (FN) potential of the base metal (FN approximately 2). Field reports also indicate the possibility...
Journal Articles
Alloy Digest (2008) 57 (4): Al-412.
Published: 01 April 2008
... cracking (SCC) per ASTM G47 with 30 day exposure is minimum 240 MPa (35 ksi). The exfoliation corrosion (EXCO) rating per ASTM G 34 is better or equal to EB. Specification Equivalents: 7040 T7451 is covered in AMS 4211, and design allowables are covered in Metallic Materials Properties Development...
Journal Articles
Alloy Digest (2007) 56 (10): Al-406.
Published: 01 October 2007
... Properties: Exfoliation corrosion, EXCO rating Better or equal to EB per ASTM G 34 Density, kg/m3 (lb/in.3) 2850 (0.103) Mechanical Properties: Tensile strength, MPa (ksi) 25 mm (1 in.) thickness 579 (84) 50 mm (2 in.) thickness 565 (82) 100 mm (4 in.) thickness 544 (79) Yield strength, MPa (ksi) 25 mm (1...
Journal Articles
Alloy Digest (2008) 57 (7): Al-415.
Published: 01 July 2008
.... It is compatible with the current surface treatment and corrosion-inhibitor methodology. A MSDS is available upon request. Corrosion Resistance: EXCO rating ASTM G47 is better or equal to EB for all thicknesses. Stress-corrosion cracking minimum in ASTM G47 in the short transverse direction is 207 MPa (30 ksi...