Alloy Digest (1984) 33 (6): SS-447.
Published: 01 June 1984
... EASTERN STAINLESS TYPE 348 is a stabilized type of stainless steel free from the chromium carbide precipitates that cause intergranular corrosion. It is recommended for welded components that cannot be annealed after welding. It also is used for parts that are heated and cooled intermittently...