Alloy Digest (1979) 28 (4): SS-363.
Published: 01 April 1979
... EASTERN STAINLESS Type 317LM is an austenitic chromium-nickel stainless steel containing low carbon (0.03% max.) and relatively high molybdenum (4.00 to 4.5%). It was developed primarily to provide more resistance to attack by sulfurous acid than is provided by competitive conventional stainless...