Alloy Digest (1984) 33 (11): SS-453.
Published: 01 November 1984
... EASTERN STAINLESS Type 317L is an austenitic chromium-nickel stainless containing low carbon (0.03% max.) and an addition of molybdenum (3.00-4.00%). This steel was developed primarily to resist more effectively the attack by sulfurous acid than is provided by some of the other competitive...
Journal Articles
Alloy Digest (1983) 32 (12): SS-437.
Published: 01 December 1983
.... Corrosion Resistance: Eastern Stainless ES-2205 provides better general corrosion resistance than AISI Types 3 l6L and 317L steels and has supertor corrosion resistance in both oxidizing and non-oxidizing acid solutions. With its higher molybdenum and chromium content. ES-2205 demonstrates superior pitting...
Journal Articles
Alloy Digest (1979) 28 (4): SS-363.
Published: 01 April 1979
... EASTERN STAINLESS Type 317LM is an austenitic chromium-nickel stainless steel containing low carbon (0.03% max.) and relatively high molybdenum (4.00 to 4.5%). It was developed primarily to provide more resistance to attack by sulfurous acid than is provided by competitive conventional stainless...