Alloy Digest (1984) 33 (2): SS-439.
Published: 01 February 1984
... EASTERN STAINLESS Type 316L is a chromium-nickel-molybdenum steel with a very low carbon content (0.03 max.) Its general resistance to corrosion is similar to AISI Type 316 but, because of its low carbon content, it has superior resistance to the formation of harmful carbides that contribute...