Alloy Digest (1961) 10 (1): Cu-1.
Published: 01 January 1961
... Duronze III is an aluminum-silicon bronze possessing high inherent hardness combined with unusual high strength. It possesses excellent corrosion resistance and exceptional wear resistance under heavy, slow moving loads. This datasheet provides information on composition, physical properties...