Alloy Digest (1961) 10 (11): Cu-109.
Published: 01 November 1961
... Duronze 707 is a tough, corrosion and wear resistant aluminum-silicon bronze, with excellent hot working and forging characteristics plus good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as...