Alloy Digest (1959) 8 (1): Cu-71.
Published: 01 January 1959
... Duronze 632 is a strong, tough and wear resistant copper alloy having corrosion resistance equal to that of copper. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well...