Alloy Digest (1996) 45 (4): Fe-109.
Published: 01 April 1996
... Durichlor 51M is a high silicon iron for corrosive services, especially in the handling of hydrochloric acid in all concentrations. It is also very resistant to most chlorine gas and many destructive chloride-containing solutions. The alloy is treated at melting by argon ladle degassing...
Journal Articles
Alloy Digest (1993) 42 (1): Fe-98.
Published: 01 January 1993
... DURICHLOR 51 SUPERCHLOR is a vacuum treated high silicon iron for corrosive services, especially in the handling of hydrochloric acid in all concentrations. It is also very resistant to most chlorine gas and many destructive chloride-containing solutions. This datasheet provides information...
Journal Articles
Alloy Digest (1955) 4 (4): Fe-7.
Published: 01 April 1955
... DURICHLOR is a high silicon iron for corrosive services, especially in the handling of hydrochloric acid in all concentrations. It is also very resistant to moist chlorine gas and many destructive chloride-containing solutions. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (12): SS-538.
Published: 01 December 1992
... Brinell Hardness 40,000 (275) 90,000 (620) 30 175 (typical) Table 2 - CORROSION RESISTANCE OF DURCOMET 5 IN OXIDIZING SERVICES 98% 160°F 180°F Nitric Acid Durcomet 5 (DV) 4 mm 4 n-w CN-7M (D20) 40 mm 42 mm CF-8 (D2) 45 mpy - CD-4M Cu 70 mw 102 mpy Durichlor 5 1 (D5 1) lw - CF-8M (D4) - 70 mw 90% Nitric...
Journal Articles
Alloy Digest (1992) 41 (11): Fe-5.
Published: 01 November 1992
... nearly universal corrosion resis- tance which makes it adaptible to many exceptionally severe services not handled by any other commercially available metal or alloy. (DURICHLOR. also manufactured by the Duriron Company.issimilarincompositiontoDURIRONbutcontains an additional 3% molybdenum. This alloy...