Alloy Digest (1966) 15 (9): TS-183.
Published: 01 September 1966
... Durax-W2 is a chromium, tungsten alloy steel recommended for normal hot working tools. It is shock and impact resistant. It is characterized by high toughness, fatigue resistance and relative ease of heat treatment. This datasheet provides information on composition, physical properties, hardness...