Alloy Digest (1962) 11 (2): SS-128.
Published: 01 February 1962
... DURALOY HT is an austenitic, non-magnetic corrosion and heat resistant alloy steel, having high resistance to thermal shock. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (1954) 3 (12): SS-21.
Published: 01 December 1954
... the same as rhe A.C.I. - HT composition in regard ro mechanical properties. The increased chromium content. however, tends to raise the strength at elevated temperatures somewhat. Under severe service conditions. this alloy is often recommended instead of the HT type, because th,e higher alloy content...