Alloy Digest (2020) 69 (1): CI-65.
Published: 01 January 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2021) 70 (4): CI-80.
Published: 01 April 2021
... Dura-Bar G2S is a high strength, pearlitic gray cast iron that is used for the production of continuous cast products. It is ideal for applications that require a combination of superior hardenability, strength, and creep resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2020) 69 (2): CI-66.
Published: 01 February 2020
... Dura-Bar G2 is a gray cast iron bar is used for continuous cast products. It is a good fit for a variety of applications due to its good machinability, wear resistance, and vibration damping properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1956) 5 (3): Ni-24.
Published: 01 March 1956
... U.S. Patent DlIice Form and Condition Rod and Bar Hot-finished Hot-finished, age-hardened Cold-drawn, as-drawn Ef$zn, age-hardened Annealed, age-hardened Physical Constants: Density, lb/cu in Specih Gravity Melting Range., F. Mean Specific Heat, BTU/lb/OF. (70-212°F.) Mean Coefficient of Thermal...