Skip Nav Destination
Close Modal
Search Results for
Dura-Bar 80-55-06
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Search Results for Dura-Bar 80-55-06
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
DURA-BAR 80-55-06: Ductile Iron
Available to Purchase
Alloy Digest (2020) 69 (7): CI-71.
Published: 01 July 2020
... Dura-Bar 80-55-06 is a ferritic-pearlitic ductile iron that is used for continuous cast products. It offers higher strength and wear resistance when compared to Dura-Bar 65-45-12, while still possessing good machinability and surface finish. This datasheet provides information on composition...
Abstract
View articletitled, <span class="search-highlight">DURA</span>-<span class="search-highlight">BAR</span> <span class="search-highlight">80</span>-<span class="search-highlight">55</span>-<span class="search-highlight">06</span>: Ductile Iron
View
PDF
for article titled, <span class="search-highlight">DURA</span>-<span class="search-highlight">BAR</span> <span class="search-highlight">80</span>-<span class="search-highlight">55</span>-<span class="search-highlight">06</span>: Ductile Iron
Dura-Bar 80-55-06 is a ferritic-pearlitic ductile iron that is used for continuous cast products. It offers higher strength and wear resistance when compared to Dura-Bar 65-45-12, while still possessing good machinability and surface finish. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on heat treating and machining. Filing Code: CI-71. Producer or source: Charter Dura-Bar, Inc.
Journal Articles
55-06 and 70-02 PEARLITIC DUCTILE DURA-BAR: Partially Pearlitic Ductile Irons
Available to Purchase
Alloy Digest (1990) 39 (8): CI-62.
Published: 01 August 1990
... 55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02...
Abstract
View articletitled, <span class="search-highlight">55</span>-<span class="search-highlight">06</span> and 70-02 PEARLITIC DUCTILE <span class="search-highlight">DURA</span>-<span class="search-highlight">BAR</span>: Partially Pearlitic Ductile Irons
View
PDF
for article titled, <span class="search-highlight">55</span>-<span class="search-highlight">06</span> and 70-02 PEARLITIC DUCTILE <span class="search-highlight">DURA</span>-<span class="search-highlight">BAR</span>: Partially Pearlitic Ductile Irons
55-06 and 70-02 Ductile Dura-Bar are continuously cast ductile irons with about 50 and 75% pearlitic microstructures, respectively. 55-06 has about the same tensile strength as SAE 1045 as-hot-rolled steel. Its maximum yield strength and elongation are equivalent to a eutectoid carbon steel. 70-02 Ductile Dura-Bar has somewhat greater tensile strength up to 3 diameter and considerably higher yield strength up through 10 diameter. The elongation of 70-02 is lower than that of 55-06 because of its reduced ferrite content. This datasheet provides information on composition, microstructure, and hardness. It also includes information on heat treating. Filing Code: CI-62. Producer or source: Federal Bronze Products Inc..