Alloy Digest (2021) 70 (10): CI-86.
Published: 01 October 2021
... Dura-Bar 60-40-18 is a ductile iron that is used for the production of continuous cast products. Its microstructure consists of nodular graphite in a fully ferritic matrix. Dura-Bar 60-40-18 is typically used for applications requiring excellent ductility and impact strength. This datasheet...