Journal Articles
Alloy Digest (1956) 5 (6): CI-14.
Published: 01 June 1956
... DUCTALLOY is a high-carbon ferrous material having high strength, high ductility, toughness and machinability. It is supplied in three grades: pearlitic grade 80, ferritic grade 60, and austenitic grade A50. This datasheet provides information on composition, physical properties, hardness...