1-12 of 12 Search Results for

Dowmetal R

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (5): Mg-17.
Published: 01 May 1955
... DOWMETAL R and DOWMETAL RC, the die casting alloys in most general use, are the 9% A1, 1% Zn magnesium alloys AZ91A and AZ91B. They combine good mechanical properties, good casting characteristics and good resistance to corrosion. A variation, designated as Dowmetal AZ91C, is used for sand...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (10): Mg-28.
Published: 01 October 1956
... AMS 4490 lizgl Alcoa 263 Elektron AZ91 Dolly Az91x &nadran CSA HGll Dowmetal R 1B General Characteristics: Apex 910 is a general die casting alloy. It possesses the desirable combination of good casting characteristics and good mechanical properties. Its minimum burning (li- quation) temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (2): Mg-15.
Published: 01 February 1955
... strength, psi (0.2 7~ ) Elongation, s in 2 F T4 TG 20000 34000 34000 10000 10000 15000 G 2 Table 2 - TYPICAL MECHANICAL PROPERTIES - PERMANENT MOLD F T4 T6 Tensile strength, psi Yield strength, psi ( .2 %r ) Elongation, % in 2 Compression ultimate strength, psi Compression yield strength, psi Shear...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (9): Mg-7.
Published: 01 September 1953
...-20 deg.. side rake of O-IO deg.. and a clearance angle of 6-10 deg. On fin- ishing operations the tool nose can be slightly rounded to secure the smoochesr. finish Broad-nose tools may hzrve the top rake reduced to about 5 deg. LO at-oid chattering parring tools should hl\fe lirtle or no top r&e...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (6): Mg-25.
Published: 01 June 1956
... weld- ing. Magnesium alloy f&r rod is used in welding and should be Dowmetal Cl composition. Corrosion Resistance: Dowmetal AZ91C does not corrode in dry air, but develops a thin gray oxide lilm in moist air. The presence of chlorides in the air of marine atmosphere increases the amount of surface...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (2): Mg-3.
Published: 01 February 1953
... tools should be ground to loo back rake, 5 side rake, 10" side cutting-edge angle, 5 end cutting-edge angle, 10' relief angle. Carbide tipped-tools should have slightly smaller rake angles in order to provide more support for the cutting ed e. Forming tools usuahy have the back rake angle r ef...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (2): Mg-8.
Published: 01 February 1954
... Strength y?o in 2" psi psi 53000 37000 9.0 70 48000 35000 11.5 200 47000 31000 20.0 iii 35000 23 25500 170 35.0 9 600 9500 6500 102.0 r I EST CARPENT R No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 D TA ON WORLD I ETALS AND ALLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w CARPENTER No. S-876...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (10): Mg-13.
Published: 01 October 1954
... RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w CARPENT R No. S-876 (A TOUGH, OIL-HARDENING. TRWLE ALLOY RYRELI CARPENTER No. 5-876 is a oidd~tium-1001~coum triple alloy steel for hard-tanpcrcd and for tough-tapered ap piications...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (5): Mg-9.
Published: 01 May 1954
... 15700 14200 8600 3700 1.83 0.067 1135 tEE% 0:18 11.5-14.0 0.249 0.077 E$yiP?n 2:: 250 300 450 7.6 15.2 19.5 40.3 :3_:22 1 Or I T CARPENT R No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 D TA ON WORLD WIDE METAL A LLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w CARPENTER No. S-876 (A TOUGH, OIL...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (1): Mg-30.
Published: 01 January 1957
... 1996 1996 ASM International chemical composition elasticity extrusion heat treatability joinability machinability physical properties tensile properties white light- MF workability All WHITE LIGHT - MF Filing Code: Mgi30 Magnesium Alloy 0 r JANUARY 1957 DIGEST - DATA ON WORLD WIDE...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (8): Mg-43.
Published: 01 August 1959
... for un6nished parts, while the Dichromate (Dow Treatment No. 7) is recommended for finished parts. Specification Equivalents: AMS 4350 & 4358 SAE 520 & 531 ASTM B91 ASTM B107 ASTM B217 Fed. QQ-M-31 Fed. WW-T-82 5 Fed. w-M-40 ME-R-6944 Alloy C General Characteristics: Correct design principles must be adhered...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (4): Mg-24.
Published: 01 April 1956
... foilowed by a Chrome Pickle and then boiling 2 hours in 5% sodium dichromate solution. Use flux for oxyacetylene gas welding- Magnesium alloy f&r rod is used in welding. Workability: Readily forged to any shape by pressing only. It is not to be hammer forged. Forgings are usually made from Q- truded...