Alloy Digest (2009) 58 (1): SA-591.
Published: 01 January 2009
... Domex 460 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-13.00 mm. The alloy meets or exceeds the requirements of S460MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...