Journal Articles
Alloy Digest (2008) 57 (7): SA-581.
Published: 01 July 2008
... Domex 315 MC is a hot-rolled, high-strength low-alloy (HSLA) steel with a fine grain structure produced through thermomechanical rolling. It is used for cold-forming operations. The alloy meets or exceeds the requirements of S315MC in EN 10149-2. This datasheet provides information on composition...