Journal Articles
Alloy Digest (2011) 60 (10): CS-167.
Published: 01 October 2011
... Dogal 300 LAD, 340 LAD, 380 LAD, 420 LAD, 460 LAD and 500 LAD are high-strength low alloyed steels intended for pressing. The designation in the name is the guaranteed minimum yield strength. Dogal steels can be zinc coated. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2015) 64 (3): CS-184.
Published: 01 March 2015
... Dogal H 700 LAD is a galvanized hot rolled steel that is microalloyed and can be cold formed. The 700 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming...
Journal Articles
Alloy Digest (2015) 64 (4): CS-186.
Published: 01 April 2015
... Dogal H 550 LAD is a galvanized hot rolled steel that is microalloyed, thermomechanically rolled, and can be cold formed. The 550 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2011) 60 (1): CS-161.
Published: 01 January 2011
... Dogal H LAD grades are microalloy steels suitable for cold forming. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: CS-161. Producer...