1-2 of 2 Search Results for

Dogal H 550 LAD

Sort by
Journal Articles
Alloy Digest (2015) 64 (4): CS-186.
Published: 01 April 2015
... Dogal H 550 LAD is a galvanized hot rolled steel that is microalloyed, thermomechanically rolled, and can be cold formed. The 550 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2011) 60 (1): CS-161.
Published: 01 January 2011
... www.asminternational.org Filing Code: Carbon Steel January 2011 CS-161 Dogal H LAD grades are microalloy steels suitable for cold forming. DOGAL® H LAD (High Strength Low Alloy Steels) DOGAL® H LAD Chemical Composition, wt (Typical) Dogal H LAD grades 420 LAD 500 LAD 550 LAD 600 LAD 650 LAD 700 LAD Carbon, max 0.10 0.10...