Alloy Digest (2023) 72 (9): TS-838.
Published: 01 September 2023
... Deutsche Edelstahlwerke Cryodur 2510 is a high-carbon, manganese-chromium-tungsten-vanadium alloy cold-work tool steel. This oil hardening type cold work tool steel offers a combination of high hardness, good wear resistance, and good cutting edge retention. This datasheet provides information...