1-1 of 1 Search Results for

Deutsche Edelstahlwerke Cryodur 2436

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2022) 71 (12): TS-834.
Published: 01 December 2022
... Deutsche Edelstahlwerke Cryodur 2436 is a high-carbon, chromium-tungsten alloy cold-work tool steel. It exhibits very high wear resistance and cutting edge retention as well as improved hardenability in comparison to Cryodur 2080. This datasheet provides information on composition, physical...