Journal Articles
Alloy Digest (2021) 70 (9): TS-817.
Published: 01 September 2021
... Deutsche Edelstahlwerke Cryodur 2249 is a medium-carbon, silicon-chromium-vanadium alloy cold-work tool steel that provides an attractive combination of high strength, high hardness, and high toughness. This datasheet provides information on composition, physical properties, hardness...