Alloy Digest (2021) 70 (3): TS-811.
Published: 01 March 2021
... Deutsche Edelstahlwerke Cryodur 2235 is a high-carbon, Cr-V, alloy cold-work tool steel that has medium hardenability and is suitable for short-run tooling requiring a combination of good wear resistance and toughness, and a keen cutting edge. This datasheet provides information on composition...