Alloy Digest (2020) 69 (12): TS-806.
Published: 01 December 2020
... Deutsche Edelstahlwerke Cryodur 2210, also known as silver steel, is a high-carbon, Cr-V, alloy cold-work tool steel that is primarily used for short-run tooling requiring low-to-medium wear resistance and very high toughness. This datasheet provides information on composition, physical properties...