... Deutsche Edelstahlwerke Cryodur 2008 is a high-carbon, chromium-vanadium alloy cold-work tool steel that is suitable for applications requiring a combination of high strength, good toughness, and good wear resistance. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2023) 72 (9): TS-838.
Published: 01 September 2023
... 2510(a) Type O1(b) 0.95 0.85 1.00 0.20 0.10 0.50 1.10 1.00 1.40 (c) 0.030 (c) 0.030 0.60 0.40 0.70 0.60 0.40 0.60 0.10 0.30 bal bal (a) Typical analysis. (b) Source: ASTM A681:2008(2015). (c) Amount not disclosed in Cryodur 2510, Deutsche Edelstahlwerke Specialty Steel GmbH & Co. KG Physical...
Journal Articles
Alloy Digest (2022) 71 (11): TS-833.
Published: 01 November 2022
... for equalization of the temperature. Soak for at least 1 h. Cool in still air. Comparable Grades Deutsche Edelstahlwerke Specialty Steel GmbH & Co. KG DIN Cryodur 2008 86CrMoV7 Copyright © 2022, ASM International®. All rights reserved. Alloy Digest: Data on Worldwide Metals and Alloys TS-833 / 2 Fig. 1 Time...
Journal Articles
Alloy Digest (2021) 70 (8): TS-816.
Published: 01 August 2021
... Edelstahlwerke Specialty Steel GmbH & Co. KG (member of Swiss Steel Group) Comparable Grades Cryodur 2242 Auestraße 4 Type L2 (UNS T61202)(a) 58452 Witten, Germany Deutsche Edelstahlwerke Specialty Tel: +49 (0) 2302 29 0 Steel GmbH & Co. KG Web: www.dew-stahl.com ASTM A681:2008(2015) All data from Cryodur 2242...
Journal Articles
Alloy Digest (2020) 69 (5): TS-792.
Published: 01 May 2020
... & Co. KG and voestalpine Böhler Edelstahl GmbH & Co KG. Comparable Grades Deutsche Edelstahlwerke ISO 4957:2018 EN ISO 4957:2018 JIS G 4404:2015 ASTM A681:2008(2015) SAE J438:2018 Cryodur 2080 X210Cr12 X210Cr12 (1.2080) SKD1 D3 (UNS T30403) D3 General Characteristics Deep depth of hardening, good non...