Alloy Digest (1969) 18 (5): Ni-145.
Published: 01 May 1969
... Deloro alloy C is a nickel base alloy designed primarily for high corrosion resistance for the chemical industry. It is used for pumps, valves, and hard facing electrodes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2021) 70 (4): Co-135.
Published: 01 April 2021
... Deloro Stellite 20 is a Co-Cr-W-C alloy. It is the most abrasion resistant standard cobalt based alloy. Its high chromium content ensures good general corrosion resistance and high-temperature oxidation resistance, while the increased tungsten level provides superior high-temperature properties...
Journal Articles
Alloy Digest (2007) 56 (4): Ni-648.
Published: 01 April 2007
... corrosion resistance in both oxidizing and reducing corrosive media. Nistelle Super C can be applied by high-velocity oxyfuel thermal spraying or plasma transfer arc welding. Nistelle is a registered trademark of Deloro Stellite Company, Inc. U.S. Patent 6,863,990 was awarded to Nistelle Super C powder...
Journal Articles
Alloy Digest (2021) 70 (8): Co-139.
Published: 01 August 2021
... cladding) can work harden to 48 HRC (550 HV). Note sourced from Stellite 21 Alloy, Deloro Stellite, 2007 Table 4 Hot hardness of undiluted weld deposit Temperature Hardness HV °C °F 347 Fig. 3 Abrasion data of various cobalt-base alloys tested per 20 68 279 ASTM G65, Procedure B. Source: Properties...
Journal Articles
Alloy Digest (2021) 70 (11): Co-142.
Published: 01 November 2021
...) ant are recommended for drilling. Information on machining expansion 10 6/K 20 200 °C 8310 sourced from Stellite 25 Alloy, Deloro Stellite, 2008. (10 6/°F) (68 392 °F) (0.300) Thermal 20 400 °C Table 1 Mechanical properties at room conductivity W/(m K) (68 752 °F) 12.2 temperature Electrical (Btu...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
... and corrosion resistance. DELORO® 50 EXV (Nickel-Base, Wear-Resistant Alloy) DELORO® 50 EXV Chemical Composition, wt (Typical) Boron 2.5 Carbon 0.5 Chromium 11 Iron 3.2 Silicon 4 Nickel bal Physical Properties: Density, 20º C (68º F), kg/m3 (lb/in.3) 7900 (0.284) Melting range, ºC (ºF) 975 1061 (1787 1941...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-422.
Published: 01 February 1993
... Elongation Strength in 1 inch Hot Hardness Ksi (MPa) percent Rockwell C 95 (656) 2 - - zi 79 (545) 3 25 - - 35 79(545-) 4 20 - - 31 62 (428) 7 82R, - - !JoRB Table 2 - ADHESIVE WEAR TEST DATA P/-M-O.1 cast - 0.1 Table 3 - ABRASIVE WEAR TEST DATA P/M- 17 cast - 35 Joining: DELORO alloys can be joined to other...
Journal Articles
Alloy Digest (1993) 42 (3): Ni-424.
Published: 01 March 1993
... DELORO 208 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-431.
Published: 01 May 1993
... DELORO 711 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... trademark. Composition, Nominal Wt., %: Cobalt 12 Iron 29 Chromium 3 Molybdenum 3 Physical Properties: Density P/M (98 lb/cu3 (g/cm3), 72°F (22 C) Theoretical PROPERTIES Tungsten 3.5 Carbon Boron 1.1 0.4 Table i - MECHANICAL PROPERTIES Other 2 Nickel Bal. Test Temp. F ( C) Room Joining: 1000 (538) DELORO...
Journal Articles
Alloy Digest (1968) 17 (6): Co-55.
Published: 01 June 1968
... DELORO STELLITE-100 is a hard and abrasion resistant alloy designed specifically for metal cutting purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1966) 15 (12): Co-49.
Published: 01 December 1966
... DELORO STELLITE-6 is a cobalt-base alloy having good resistance to wear and shock along with excellent corrosion resistance and high temperature strength. It is recommended for steam and chemical valves. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1969) 18 (1): Co-57.
Published: 01 January 1969
... DELORO STELLITE 4 is a cobalt-base alloy having high wear resistance, good high temperature strength. It is a machinable casting alloy recommended for hot extrusion and pressing dies, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1965) 14 (5): Co-44.
Published: 01 May 1965
... Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides...
Journal Articles
Alloy Digest (1997) 46 (7): SS-688.
Published: 01 July 1997
... on corrosion and wear resistance as well as joining. Filing Code: SS-688. Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys fracture toughness...
Journal Articles
Alloy Digest (2006) 55 (8): Co-113.
Published: 01 August 2006
... trademarks of Deloro Stellite Company, Inc. Mechanical Properties: Hardness, plasma transferred arc (PTA) 45 50 all weld deposit, HRC Charpy impact test results are shown in Fig. 2. Tribaloy T-401 shows better toughness than any of the other alloys in the Laves phase alloy family. Weldability: Tribaloy T-401...
Journal Articles
Alloy Digest (1996) 45 (10): Co-100.
Published: 01 October 1996
...: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys hardness microstructure Tribaloy alloy T-900 wear resistance DATA ON WORLD WIDE METALS AND ALLOYS...
Journal Articles
Alloy Digest (2006) 55 (10): Co-114.
Published: 01 October 2006
... phase particles to promote wear resistance while improving corrosion and oxidation resistance over T400. Tribaloy and Stellite are registered trademarks of Deloro Stellite Company, Inc. Weldability: Compared with alloy T-400, T-400C can be weld deposited with plasma transfer arc welding with fewer...
Journal Articles
Alloy Digest (1997) 46 (6): Ni-528.
Published: 01 June 1997
... for nuclear plant applications. These alloys have been used in Japanese comnxmial nuclear power plant service for several years. Nucalloy. Stellite@. Debra@, and Stoody@ are registered trademarks of Stoocly Deloro Stellite. Inc. Nucalloy alloys are covered under U.S. Patent No. 4404.049. Chemical Composition...
Journal Articles
Alloy Digest (1994) 43 (12): SS-576.
Published: 01 December 1994
... should be a minimum of 36 Rockwell C. *Weld consumable for CAS Tungsten Arc Welding. Table 1 - WELDABKLIN Suggested welding parameters for Norem 02 Alloy. Automatic gas nmgsten arc welding using 0.045 diameter wire. Variable Value Position Preheat current Gq-4 hary Background Voltage (volts) primary...