Alloy Digest (2021) 70 (4): Co-135.
Published: 01 April 2021
... Deloro Stellite 20 is a Co-Cr-W-C alloy. It is the most abrasion resistant standard cobalt based alloy. Its high chromium content ensures good general corrosion resistance and high-temperature oxidation resistance, while the increased tungsten level provides superior high-temperature properties...
Journal Articles
Alloy Digest (2021) 70 (8): Co-139.
Published: 01 August 2021
... cladding) can work harden to 48 HRC (550 HV). Note sourced from Stellite 21 Alloy, Deloro Stellite, 2007 Table 4 Hot hardness of undiluted weld deposit Temperature Hardness HV °C °F 347 Fig. 3 Abrasion data of various cobalt-base alloys tested per 20 68 279 ASTM G65, Procedure B. Source: Properties...
Journal Articles
Alloy Digest (1965) 14 (5): Co-44.
Published: 01 May 1965
... Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides...
Journal Articles
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
...: Stellite Coatings. Producer or Source: Stellite Coatings Copyright © ASM International® 2011 2011 ASM International chemical composition DELORO 15 ALLOYS DELORO 21 ALLOYS DELORO 22 ALLOYS DELORO 25 ALLOYS hardness molds nickel powder physical properties powder metal products DATA...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
... resistance as well as powder metal forms. Filing Code: Ni-683. Producer or source: Deloro Stellite Company Inc. Producer or Source: Deloro Stellite Company Inc. Copyright © ASM International® 2010 2010 ASM International abrasion resistance chemical composition corrosion-resistant alloys...
Journal Articles
Alloy Digest (1968) 17 (6): Co-55.
Published: 01 June 1968
... DELORO STELLITE-100 is a hard and abrasion resistant alloy designed specifically for metal cutting purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1969) 18 (1): Co-57.
Published: 01 January 1969
... DELORO STELLITE 4 is a cobalt-base alloy having high wear resistance, good high temperature strength. It is a machinable casting alloy recommended for hot extrusion and pressing dies, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1966) 15 (12): Co-49.
Published: 01 December 1966
... DELORO STELLITE-6 is a cobalt-base alloy having good resistance to wear and shock along with excellent corrosion resistance and high temperature strength. It is recommended for steam and chemical valves. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1996) 45 (11): Co-101.
Published: 01 November 1996
... information on corrosion and wear resistance. Filing Code: CO-101. Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition compressive strength corrosion-resistant alloys...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... and wear resistance as well as machining and joining. Filing Code: Ni-435. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition DELORO 716 PM hardness high-temperature alloys...
Journal Articles
Alloy Digest (1969) 18 (5): Ni-145.
Published: 01 May 1969
... as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-145. Producer or source: Deloro Stellite Ltd. Producer or Source: Deloro Stellite Ltd Copyright © ASM International® 1996 1996...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-422.
Published: 01 February 1993
... resistance as well as machining and joining. Filing Code: Ni-422. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition DELORO N-6 PM hardness joinability machinability physical...
Journal Articles
Alloy Digest (1994) 43 (12): SS-576.
Published: 01 December 1994
... the aim NOREM 02 chemistry given in Table 1. Table 3 - GALLING WEAR OF GTA WELD OVERLAYS Surface Damage (mm) at Indicated Stress (ksi) Tests in Air Tests in Water Alloy 20 40 60 20 40 60 Deloro 40/nickel-base 37.1 41.3 50.0 17.3 34.7 40.0 Deloro 50/nickel-base 38.6 NT 76.0 14.7 26.4 34.7 Stellire 2l...
Journal Articles
Alloy Digest (1996) 45 (12): SS-662.
Published: 01 December 1996
... provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on corrosion and wear resistance as well as joining. Filing Code: SS-662. Producer or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc...
Journal Articles
Alloy Digest (1997) 46 (2): SS-672.
Published: 01 February 1997
... or source: Stoody Deloro Stellite Inc. Producer or Source: Stoody Deloro Stellite Inc. Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys hardness joinability physical properties Tristelle alloy TS-3 wear resistance thermal...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-431.
Published: 01 May 1993
... information on high temperature performance as well as machining and joining. Filing Code: Ni-431. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition creep properties DELORO 711 PM...
Journal Articles
Alloy Digest (2007) 56 (4): Ni-648.
Published: 01 April 2007
... includes information on corrosion resistance as well as surface treatment and powder metal forms.Filing Code: Ni-648. Producer or source: Deloro Stellite Company Inc. Producer or Source: Deloro Stellite Company Inc. Copyright © ASM International® 2007 2007 ASM International chemical...
Journal Articles
Alloy Digest (1993) 42 (10): Co-94.
Published: 01 October 1993
..., and tensile properties. It also includes information on wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: CO-94. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (2006) 55 (10): Co-114.
Published: 01 October 2006
.... It also includes information on corrosion and wear resistance as well as casting, joining, and powder metal forms. Filing Code: CO-114. Producer or source: Deloro Stellite Company Inc. Producer or Source: Deloro Stellite Company Inc. Copyright © ASM International® 2006 2006 ASM International...
Journal Articles
Alloy Digest (2019) 68 (12): Co-87.
Published: 01 December 2019
... properties. It also includes information on wear resistance as well as heat treating, machining, and joining. Filing Code: Co-87. Producer or source: Deloro Stellite Inc.. Originally published December 1993, corrected December 2019. Producer or Source: Deloro Stellite Inc. Copyright © ASM International...