Alloy Digest (1977) 26 (11): SA-338.
Published: 01 November 1977
... DYNA-LOY HS-32 is a cold-drawn high-strength alloy steel developed for those applications that require a minimum hardness of Rockwell C 32. Its chemical composition permits maximum machinability and improved surface finish at a guaranteed minimum tensile strength of 150,000 psi as supplied. Thus...