Alloy Digest (1996) 45 (3): SS-5.
Published: 01 March 1996
... DURIMET 20 is a special austenitic stainless steel alloy of nickel, chromium, molybdenum, and copper. It is highly resistant to hot and cold strong acids and is supplied in the form of castings to the grade CN7M. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1993) 42 (2): SS-540.
Published: 01 February 1993
.... In the more dilute COtMXIlUations of sulfuric acid. it is superior to Durimet 20 (CN-7M). The alloy is less resistant to deaerated sulfuric acid thsn it is to aerated acid Aeration or the presence of oxidizing contami- nants such as nitric acid, fenic sulfate or cupric sulfate would extend the range...