Skip Nav Destination
Close Modal
Search Results for
DURANICKEL
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-5 of 5 Search Results for
DURANICKEL
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1953) 2 (1): Ni-2.
Published: 01 January 1953
... DURANICKEL, formerly known as Z-Nickel, is an age-hardenable nickel alloy having high strength and high corrosion resistance in addition to high heat resistance. It is magnetic at room temperature in all conditions. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
DURANICKEL, formerly known as Z-Nickel, is an age-hardenable nickel alloy having high strength and high corrosion resistance in addition to high heat resistance. It is magnetic at room temperature in all conditions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-2. Producer or source: Huntington Alloy Products Division, An INCO Company.
Journal Articles
Alloy Digest (1956) 5 (3): Ni-24.
Published: 01 March 1956
... DURANICKEL R is an age-hardenable nickel alloy having high strength and high corrosion resistance. It is magnetic at room temperature in all conditions. It is recommended for improved machinability over standard Duranickel. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
DURANICKEL R is an age-hardenable nickel alloy having high strength and high corrosion resistance. It is magnetic at room temperature in all conditions. It is recommended for improved machinability over standard Duranickel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-24. Producer or source: The International Nickel Company Inc..
Journal Articles
Alloy Digest (1963) 12 (6): Ni-83.
Published: 01 June 1963
... DURANICKEL Alloy 301 is a wrought, age-hardenable nickel alloy having high strength, high corrosion and heat resistance. It is recommended for springs, diaphrams, bearings, pump and valve parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and...
Abstract
View article
PDF
DURANICKEL Alloy 301 is a wrought, age-hardenable nickel alloy having high strength, high corrosion and heat resistance. It is recommended for springs, diaphrams, bearings, pump and valve parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-83. Producer or source: The International Nickel Company Inc..
Journal Articles
Alloy Digest (1967) 16 (8): Ni-126.
Published: 01 August 1967
... PERMANICKEL alloy 300 is an age-hardenable high-nickel alloy similar to DURANICKEL alloy 301 in its strength and corrosion resistance, but having higher thermal and electrical conductivity. The alloy is somewhat difficult to heat treat, and DURANICKEL alloy 301 is recommended in preference to it...
Abstract
View article
PDF
PERMANICKEL alloy 300 is an age-hardenable high-nickel alloy similar to DURANICKEL alloy 301 in its strength and corrosion resistance, but having higher thermal and electrical conductivity. The alloy is somewhat difficult to heat treat, and DURANICKEL alloy 301 is recommended in preference to it except for applications requiring its superior conductivity or magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-126. Producer or source: The International Nickel Company Inc..
Journal Articles
Alloy Digest (1960) 9 (12): Ni-63.
Published: 01 December 1960
... against other hardened materials such as hardened steel, against itself, or ocher age-hardenable nickel alloys such as Ioconel X , K Monel, or Duranickel. If it is used against softer materials, galling is likely to occur. Forms Available: Castings Applications: Cast parts in processing equipment for...
Abstract
View article
PDF
S Inconel is a nickel-base alloy recommended for applications requiring resistance to wear and galling in addition to high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-63. Producer or source: The International Nickel Company Inc..