Alloy Digest (1955) 4 (9): TS-37.
Published: 01 September 1955
... DURAMOLD A is the low-carbon 4 1/2% chromium type of air-hardening hobbing die steel. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-37. Producer or source...
Journal Articles
Alloy Digest (1969) 18 (7): TS-221.
Published: 01 July 1969
... DURAMOLD N is a low-carbon, nickel-chromium type of plastic-molding die steel capable of developing a deep carburized case combined with exceptional core strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1965) 14 (9): TS-169.
Published: 01 September 1965
... DURAMOLD-B is a low carbon, low alloy carburizing grade of steel recommended for hobbed plastic molds and dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as...
Journal Articles
Alloy Digest (1957) 6 (6): TS-59.
Published: 01 June 1957
... regards hobabiliy by Gshing the forging at a high temperature. This is due to the fact that the resulting larger grain sire will produce a lower Brinell hardness. Specification Equivalents: AISI Tppe Pl sm Type Pl Duramold C Bethlehem Ivfirromold Crusca Cold Hubbing Carpenter Crucible General...