1-1 of 1 Search Results for

DURA-BAR G1A GLASS MOLD IRON

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1990) 39 (7): CI-61.
Published: 01 July 1990
... DURA-BAR G1A alloyed iron is engineered for the glass mold industry. It is produced by continuous casting which results in fine graphite flake size and size and fine matrix structure. This datasheet provides information on composition, microstructure, and hardness. It also includes information...