Alloy Digest (1953) 2 (2): Mg-3.
Published: 01 February 1953
... DOWMETAL M is a manganese type magnesium base alloy which does not respond to hardening heat treatment, but is recommended where maximum formability and weldability are desired. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1955) 4 (5): Mg-17.
Published: 01 May 1955
... the Dichromace (Dow Chemical Treatment No. 7) is recommended for finished parts. Complete protecrion is achieved by means of anodic treatment-either H.A.E. or Dow Chemical Treatment No. 17. Specification Equivalents: SAE 501 & 501A ASTM B93, AZ91A & AZ91B ASTM B94, AB91A & AZ91B Fed. w-M-56, AZ91 Fed. QQ-M-38...
Journal Articles
Alloy Digest (1953) 2 (9): Mg-7.
Published: 01 September 1953
... Extruded tubing Federal WW-T-825 SAE 52 ASTM B217-i9TZ~lB Sheet AMS 4375 SAE 510 ASTM B90-5 IT-AZ31A Federal QQ-M-44 Typical Radii at Temperarute 70 deg. F 300 deg. F 400 deg. F. 4 li2t 1.2t 8r 4 l/2-6t General Characteristics: Donmetal FS-1 is of higher purity than Dowmetal FS. Both are general purpose...
Journal Articles
Alloy Digest (1955) 4 (12): Mg-21.
Published: 01 December 1955
...- sition as the alloy welded. Specification Equivalents: This alloy is governed by the same specifications as govern the alloy produced under the trade-name of ZREl. ASTM B80-54T Military MIL-M-9433 General Characteristics: This alloy possesses good resistance to creep up to about 500°F. It is virtually...
Journal Articles
Alloy Digest (1955) 4 (2): Mg-15.
Published: 01 February 1955
...-AMlOOA Alcoa 240 SAE 502 Air Force 11348 Federal w-M-55 General Characteristics: Dowmetal G is a heat treatable magnesium casting type alloy suitable for permanent mold and sand castings. It responds favorably to an age-hardening heat treat- ment and has good casting properties. It is generally...
Journal Articles
Alloy Digest (1956) 5 (7): Mg-26.
Published: 01 July 1956
... International® 1996 1996 ASM International chemical composition creep resistance Dowmetal HZ32XA elasticity heat treatability high-temperature alloys joinability machinability physical properties tensile properties I Filing Code: Mg-26 m am Magnesium Alloy ImmfiU WEST ci DOWMETAL HZ32XA JULY...
Journal Articles
Alloy Digest (1956) 5 (6): Mg-25.
Published: 01 June 1956
... B80-54T Federal QQ-M-56 General Characteristics: This alloy is a heat treatable casting type magnesium alloy. It is used for both sand and permanent mold castings especially where soundness and pressure tight- ness are required. This alloy has better castabiliy than Dowmetal H and has comparable...
Journal Articles
Alloy Digest (1954) 3 (10): Mg-13.
Published: 01 October 1954
... for tished parts. Specification Equivalents: ASTM B93-AZ92A; B80-AZ92A; B199-AZ92A Alcoa 260 Army 57-74-1 and 57-74-2 SAP 500 and 503 AMS 4434 and 4484 Federal QQ-M-55 and QQ-M-56 Alloy AZ92 MIL-R-6944 General Characteristics: Dowmeral C is a heat treatable casting type magnesium alloy. It is used for both...
Journal Articles
Alloy Digest (1954) 3 (5): Mg-9.
Published: 01 May 1954
... Specifications: ASc4S~~2~593-AZ63A and BSO-AZ63A SAE 50 QQ-M-56 camp. AZ63 AMS 4420 and 4422 and 4424 Readily welded by the inert gas electric-arc method. With the inert gas, no flux is necessary and rhere is no danger of flux entrapment. Arc welding provides a fast method of producing high strength welds...
Journal Articles
Alloy Digest (1954) 3 (2): Mg-8.
Published: 01 February 1954
... © ASM International® 1996DOI: 10.31399/asm.ad.mg0008 MachinabiITty: Bxa?IIent marhinlhiliy racing. use high cuaing speeds, modaace feeds and depths of cut. Iarge top and side rake, aud ample chip cIeamnce. Keep m=ifJg &a zhvD and kmlacalItimes. HAS. Iark rooI.5 for rough cutting require 8-10 deg...
Journal Articles
Alloy Digest (1952) 1 (1): Mg-1.
Published: 01 September 1952
... (6sZl2v) 0.0000145 PROPERTIES: Tabk 1 ultimate Talsik ~fJas+ Talsile Yield tion Form sire conditim (1) S-Mb lo 2 %-IQ- 1000 psi 1OOOpSi Pacart 1000 psi Typ. Min. Typ. Min. Typ. Mio. Typ. Min. Less tbim -F 49 43 38 42 2 12 5 32 27 Rods, 2 -TS 51 45 10 4 35 30 Bars 2 atad m -F 40 43 38 31 12 5 30 26 Solid...
Journal Articles
Alloy Digest (1960) 9 (1): Mg-44.
Published: 01 January 1960
... in welding and should be Dowmetal Cl composition. DOI: 10.31399/asm.ad.mg0044 Copyright © ASM International® 1996 Specification Equivalents: ASTM B91-%T QQ-M-40 Alloy TA54A SAE 53 Corrosion Resistance: It does not corrode in dry air, but develops a thin gray oxide film in moist air. The presence of chlo...
Journal Articles
Alloy Digest (1956) 5 (10): Mg-28.
Published: 01 October 1956
... Treat- ment No. 7) IS recommended for finished parts. Complete protection is achieved by means of anodic treatment - either H. A.E. or Dow Chemical Treatment No. 17. ecification Equivalents: SAE 501 ASTM B93, AZ9lA ASTM B94, AZ9lA & AZ9 Fed. QQ-M-56, AZ91 Ei EFE-M-16 MILM-4204 Navy 46Mll Army 57-74-3...
Journal Articles
Alloy Digest (1959) 8 (8): Mg-43.
Published: 01 August 1959
... for un6nished parts, while the Dichromate (Dow Treatment No. 7) is recommended for finished parts. Specification Equivalents: AMS 4350 & 4358 SAE 520 & 531 ASTM B91 ASTM B107 ASTM B217 Fed. QQ-M-31 Fed. WW-T-82 5 Fed. w-M-40 ME-R-6944 Alloy C General Characteristics: Correct design principles must be adhered...