1-12 of 12

Search Results for DOGAL FORM

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2010) 59 (10): CS-158.
Published: 01 October 2010
... DOGAL 200 AND DOGAL FORM mild steels can be used for applications ranging all the way from simple pressing up to advanced drawing and stretch forming. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, joining...
Journal Articles
Alloy Digest (2011) 60 (8): CS-166.
Published: 01 August 2011
... on surface qualities as well as forming, joining, and surface treatment. Filing Code: CS-166. Producer or source: SSAB Hardox Corporation. Producer or Source: SSAB Hardox Corporation Copyright © ASM International® 2011 2011 ASM International bend strength chemical composition DOGAL 600 CP...
Journal Articles
Alloy Digest (2010) 59 (11): CS-159.
Published: 01 November 2010
... limit curves are shown in Fig. 1. General Characteristics: Dogal 500 DP is an extra high-strength steel that is hot-dip galvanized for corrosion protection. Dogal DP steels are easy to cold form and excellent for stretch forming and roll forming. The steel grade is supplied in accordance with prEN 10336...
Journal Articles
Alloy Digest (2010) 59 (12): CS-160.
Published: 01 December 2010
... electrode forces and longer weld times are used. Formability: Forming limit curves are shown in Fig. 1. General Characteristics: Dogal 600 and 800 DP are extra and ultra high-strength steels that are hot dip galvanized for protection against corrosion. Dogal DP grades are dual phase steels that contain...
Journal Articles
Alloy Digest (2011) 60 (10): CS-167.
Published: 01 October 2011
... the conventional fusion welding methods can be used. For spot welding it is recommended to use increased electrode force and weld time to optimize the weld quality. General Characteristics: Dogal LAD grades are micro-alloyed cold-forming steels that derive their high strength from the addition of very small...
Journal Articles
Alloy Digest (2011) 60 (3): CS-162.
Published: 01 March 2011
... Formability properties Steel grade Stretch- forming, H/d Deep drawing, LDR Inside radius for 90° bend (t=thickness) Flanging Burr in Burr out Dogal 800 DPX 0.33 2.05 0.9·t 1.3 1.25 General Characteristics: Dogal 800 DPX is an ultra-high-strength steel that is hot dip galvanized for protection against...
Journal Articles
Alloy Digest (2011) 60 (4): CS-163.
Published: 01 April 2011
... Steel grade Stretch- forming, H/d Deep drawing, LDR Inside radius for 90° bend (t=thickness) Flanging Burr in Burr out Dogal 1000 DPX 0.25 1.9 2.5·t 1.25 1.2 General Characteristics: Dogal 1000 DPX is an ultra-high-strength steel that is hot dip galvanized for protection against corrosion. Dogal DPX...
Journal Articles
Alloy Digest (2011) 60 (1): CS-161.
Published: 01 January 2011
... Dogal H LAD grades are microalloy steels suitable for cold forming. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming, heat treating, joining, and surface treatment. Filing Code: CS-161. Producer...
Journal Articles
Alloy Digest (2015) 64 (3): CS-184.
Published: 01 March 2015
... Dogal H 700 LAD is a galvanized hot rolled steel that is microalloyed and can be cold formed. The 700 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming...
Journal Articles
Alloy Digest (2015) 64 (4): CS-186.
Published: 01 April 2015
... Dogal H 550 LAD is a galvanized hot rolled steel that is microalloyed, thermomechanically rolled, and can be cold formed. The 550 signifies the minimum yield strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2011) 60 (2): SA-620.
Published: 01 February 2011
... DOGAL API 2W GRADE 50 is thermomechanical control processed plate produced to meet specifications for API 2W Grade 50 Steel. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-620...
Journal Articles
Alloy Digest (2010) 59 (1): SA-613.
Published: 01 January 2010
... Docol Roll 800 and 1000 are advanced high-strength controlled steels designed for roll forming. This datasheet provides information on composition, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-613. Producer or source: SSAB Swedish...