Alloy Digest (2011) 60 (3): CS-162.
Published: 01 March 2011
... Dogal 800 DPX is a high strength steel with a microstructure that contains ferrite, which is soft and formable and martensite, which is hard and contributes to the strength of the steel. The designation relates to the lowest tensile strength. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2011) 60 (4): CS-163.
Published: 01 April 2011
.... Table 1 Mechanical properties (transverse to rolling direction) Steel grade 0.2% yield strength, MPa (ksi) Tensile strength, MPa (ksi) Elongation min, % Dogal 1000 DPX 800 1000 (115 145) 1000 1200 (145 175) 6 Weldability: Dogal 1000 DPX can be welded with all conventional fusion welding methods...