Journal Articles
Alloy Digest (2010) 59 (10): CS-158.
Published: 01 October 2010
... DOGAL 200 AND DOGAL FORM mild steels can be used for applications ranging all the way from simple pressing up to advanced drawing and stretch forming. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, joining...
Journal Articles
Alloy Digest (2011) 60 (2): SA-620.
Published: 01 February 2011
... DOGAL API 2W GRADE 50 is thermomechanical control processed plate produced to meet specifications for API 2W Grade 50 Steel. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-620...
Journal Articles
Alloy Digest (2011) 60 (10): CS-167.
Published: 01 October 2011
.... The heating can affect the zinc coating, which can result in poor appearance and deterioration of the corrosion properties. If the material is eventually heated, the temperatures should be limited to maximum temperature 200 °C (392 °F). Weldability: Dogal LAD offer excellent welding characteristics...
Journal Articles
Alloy Digest (2010) 59 (12): CS-160.
Published: 01 December 2010
... Dogal 600 and 800 DP are high-strength steels with a microstructure that contains ferrite, which is soft and formable, and martensite, which is hard and contributes to the strength of the steel. The designation relates to the lowest tensile strength. This datasheet provides information on...
Journal Articles
Alloy Digest (2011) 60 (1): CS-161.
Published: 01 January 2011
.... The heating can affect the zinc coating which can result in poor appearance and deterioration of the corrosion properties. If the material is heated, the temperature should be limited to a maximum of 200 ºC (392 ºF). Weldability: Dogal H LAD offer excellent welding characteristics. All the...
Journal Articles
Alloy Digest (2011) 60 (3): CS-162.
Published: 01 March 2011
... Dogal 800 DPX is a high strength steel with a microstructure that contains ferrite, which is soft and formable and martensite, which is hard and contributes to the strength of the steel. The designation relates to the lowest tensile strength. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2011) 60 (4): CS-163.
Published: 01 April 2011
... Dogal 1000 DPX is a high strength steel with a microstructure that contains ferrite, which is soft and formable, and martensite, which is hard and contributes to the strength of the steel. The designation relates to the lowest tensile strength. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2011) 60 (8): CS-166.
Published: 01 August 2011
... 10 140 120 Z200 14 200 170 Z275 20 275 235 (a) The values are calculated on the basis of the minimum values for the triple-spot test (1 m = 7.14 g/m2). Surface Treatment. Surface-treated Dogal steels are provided with chemical and/or oiling passivation as surface protection. The chemical passivation...