1-1 of 1 Search Results for

DOCOL 140DP

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (3): SA-531.
Published: 01 March 2004
... Docol 140DP is an ultrahigh-strength steel (0.15C-0.50Si) that is used for many transportation products. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on machining and joining. Filing Code: SA-531. Producer or source...