Alloy Digest (2004) 53 (1): SA-528.
Published: 01 January 2004
... Docol 130M is a high strength cold forming steel that is used for transportation and structural products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on joining. Filing Code: SA-528. Producer or source...