Publisher: Journals Gateway
Alloy Digest (2014) 63 (12): SA-715.
Published: 01 December 2014
... Docol 1000 DPZE is a high-strength steel with a microstructure that contains ferrite, which contributes to good formability, and martensite, which is hard and contributes to the strength of the material. These steels are designed according to their lowest tensile strength. DP stands for dual phase...